Alloy M25 (UNS C17300)offers the strength properties of Alloy 25 with the added benefit of being "free machining." Alloy M25 rod and wire contain a small amount of lead to provide an alloy tailored for automatic machining operations. Lead promotes formation of finely divided chips, thus extending cutting tool life.
12' Random Lengths Condition H (Hardened) Specifications: CDA 173 ASTM B196 UNS C17300 Nominal Composition: Copper: 97.7% Beryllium: 1.9% Lead: 0.4% Also available in condition A (annealed).